Lots of stringing but as I understand that’s normal for TPU. Printed at 225⁰C on a 30⁰ bed, stock Ender 3 S1. 0 retraction, 0.93 flow, 35mm/s for most speeds
Lots of stringing but as I understand that’s normal for TPU. Printed at 225⁰C on a 30⁰ bed, stock Ender 3 S1. 0 retraction, 0.93 flow, 35mm/s for most speeds
How would you suggest going about aggressively dehydrating it?
Run it in a dehydrater for 6h prior and during print